A wall thickness that falls short of the required specification means, first and foremost, that a measured value deviates from the required specifications. As wall thickness is usually both technically
A failed test result means, first and foremost, that at least one measured parameter did not meet the specified requirements. This indicates a deviation from the specified requirements. However, the
Both results are relevant, as they test different characteristics. The on-site leak test assesses the refurbished pipe system as a whole under actual installation conditions. Among other things, it checks
A failed test result initially simply means that a requirement stipulated in the contract, by technical specifications or by standards has not been met. Whether this constitutes a defect leading
Flexural strength describes the load-bearing capacity of the material up to the point of failure. It therefore indicates the forces that the pipe liner can withstand before damage occurs. If
The flexural modulus describes the stiffness of a pipe liner. Put simply, it indicates how much the material deforms under load. The higher the flexural modulus, the less a test
A slight undershoot of mechanical performance values generally constitutes a deviation from the required minimum values. If the performance values from a DIBt approval are contractually agreed, these must generally
If test results are inconclusive or require further technical assessment, supplementary investigations may be advisable. Typical reasons for this include unusual mechanical properties, indications of incomplete curing, or the question
If contractually agreed minimum requirements are not met, this initially constitutes a deviation from the performance due and therefore, in principle, a defect. However, any further assessment should take the
The pressure pipe load cycle test is a practical testing method for pressure pipe systems. Its distinctive feature is that it is the only system test of its kind to